用分段活化—浮选法回收某锌浸渣中的银

Application of Segmented Activation - Flotation to Silver Recover from a Zinc Leach Residue

  • 摘要: 某锌冶炼厂酸浸渣含银150~250 g/t,其中硫化银和单质银等可回收银仅占64.01%,银矿物粒度细且赋存形态复杂。针对该难选冶炼渣,采用分段活化—浮选工艺回收该酸浸渣中的银,并且控制矿浆Zn2+含量小于30 g/L,闭路试验可获得银精矿含银4 466.99 g/t、银回收率57.67%,相比现场银精矿品位及回收率均有较大幅度提升。

     

    Abstract: The acid leaching residue of a zinc smelter contained Ag 150-250 g/t. Silver sulfide, elemental silver and other recoverable silver accounted for only 64.01%. The silver mineral size was fine and the occurrence form was complex. The silver in the acid leaching slag was recovered by the process of Segmented activation - flotation, and the content of Zn2+ in the pulp was controlled to be less than 30 g/L. Silver concentrate can be obtained by closed - circuit test with Ag grade 4 466.99 g/t and Ag recovery 57.67%, which was greatly improved compared with the grade and recovery of the on-site silver concentrate.

     

/