耐低温脂肪酸类捕收剂浮选内蒙古某高含泥石英型萤石矿试验研究

Mineral Processing Study on a High-mud Quartz-type Fluorite Ore From Inner Mongolia Using a Low-temperature-resistant Fatty Collector

  • 摘要: 对内蒙古某含CaF2 41.14%、SiO2 42.59%、CaCO3 1.68%的高含泥石英型萤石矿进行了选矿工艺优化试验研究。根据矿石性质,进行了中矿顺序返回和精选Ⅰ中矿扫选后抛尾两种原则工艺流程的闭路试验研究,萤石粗选时,采用碳酸钠作调整剂,水玻璃作抑制剂,耐低温的改性脂肪酸类BK410B作捕收剂将萤石矿物浮出,获得萤石粗精矿;萤石粗精矿再磨后,采用酸化水玻璃作抑制剂8次精选,得到萤石精矿。通过中矿顺序返回和精选Ⅰ中矿扫选后抛尾两种试验方案的工艺流程和闭路试验指标的对比分析,最终确定了精选Ⅰ中矿扫选后抛尾的工艺流程,闭路试验获得CaF2品位97.68%、CaCO3品位0.55%、SiO2品位1.38%、CaF2回收率95.72%的萤石精矿。新工艺实现了矿石中萤石矿物的高效回收。

     

    Abstract: Mineral processing study was carried out on a high-mud quartz-type fluorite ore with CaF2 content of 41.14%, SiO2 content of 42.59% and CaCO3 content of 1.68% from Inner Mongolia. The two processes of flotation of sequential return of the middlings and discarding the tailings of scavenging from the middlings of cleaning Ⅰ were proposed based on the characteristics of the ore property, firstly, the fluorite rough concentrate was obtained by flotation with sodium carbonate and water glass as modifier, collector BK410B, a kind of low-temperature resistance modified fatty acid collector, and then the fluorite minerals were recovered by flotation separation from the fluorite rough concentrate after being reground with acidized water glass as modifier and the fluorite concentrate was obtained. The comparison tests were conducted by adopting two technological processes of sequential return of the middlings and discarding the tailings of scavenging from the middlings of cleaning Ⅰ. Finally, the flowsheet of discarding the tailings of scavenging from the middlings of cleaning Ⅰ was determined, and the results of closed-circuit test were obtained the fluorite concentrate with grading 97.68% CaF2, 0.55% CaCO3, 1.38% SiO2 and CaF2 recovery of 95.72%. It can be achieved efficient recovery of the fluorite minerals in new process of the ore.

     

/

返回文章
返回