  • 摘要: 水体中氟化物含量超标一直是全球关注的环境问题之一,使用含钙物质生成氟化钙沉淀法,出水浓度一般在8~9 mg/L,不能满足饮用水中含氟低于1.5 mg/L的世卫标准。为此,本文基于机械力活化的概念,使用行星磨球磨钙铝氢氧化物合成加藤石材料Ca3Al2(OH)12,通过OH-与F-离子交换的新脱氟机理,实现了饮水达标的深度脱氟。在Ca:Al摩尔比为3:2、球磨1 h、转速为500 r/min的条件下,制备的材料可将氟离子浓度从10 mg/L降到0.32 mg/L。用高岭石代替氢氧化铝也能实现类似的深度脱氟,为含氟废水的高度净化提供了新的思路和可行性。

     

    Abstract: Excessive fluoride content in water has always been one of the environmental issues of global concern. The calcium fluoride precipitation method produced by calcium-containing substances with the effluent concentration of 8-9 mg/L cannot meet the WHO standard that the fluorine content in drinking water is less than 1.5 mg/L. Based on the concept of mechanochemical activation, the goal of deep defluoridation of drinking water up to standard has been achieved by the Ca3Al2(OH)12 synthesized by grinding calcium aluminum hydroxide using planetary milling balls, which is based on a new defluorination mechanism of OH- and F- exchange. The prepared material can reduce the fluoride ion concentration from 10mg/L to 0.32 mg/L under the condition of the molar ratio of Ca: Al being 3:2, grinding time of 1h and the stirred speed of 500 r/min. Substituting kaolinite for aluminum hydroxide can also achieve similar deep defluorination, which provides new ideas and feasibility for the high purification of fluorine-containing wastewater.

     

/

返回文章
返回